Stamping process · Razor blades

How Are Razor Blades Made? The Strip Punching Stage and Its Coil Line

A razor blade begins as a coil of thin stainless strip. Here is every step from strip to blade, why the strip is punched first and kept in one piece, and the coil line with a pallet decoiler, a servo pull feeder and a rewinder.

Process guide · 14 min read · 1 video · 1 calculator

GCH-200 high-speed double servo feeder fitted to a C-frame press, with its strip guide rollers at the entry
A GCH-200 high-speed double servo feeder fitted to a C-frame press.
6 stepsStrip, punch, harden, grind and hone, coat, cut.
60 m/minReference feed speed of the GCH double servo feeder.
±0.02 mmFeeding accuracy reference of the GCD high-speed servo feeder.
0.03–0.3 mmThickness range of the HENLI 6-Hi thin strip leveler.

Every razor blade, double-edge or cartridge, starts the same way: as a coil of thin, narrow stainless steel strip. Long before it is sharp, the strip goes through a press that punches the holes and slots the blade needs.

This guide follows a blade from coil to package: what it is made of, the six manufacturing steps, why punching comes before hardening, and the coil line that does it, from a flat pallet decoiler to a servo feeder that pulls the strip out of the die and a rewinder. A calculator checks the strip speed and the blanks per coil for your own strip.

The short answer

Razor blades are made from a coil of thin martensitic stainless steel strip. First the strip is punched on a press with the slots, holes and notches the blade needs, while it is still soft and in one piece: a flat pallet decoiler pays the coil off, a high-speed single or double servo feeder pulls the punched strip out of the die, and a rewinder winds it up again. The strip is then hardened by heating, quenching and tempering, both long edges are ground and honed to a fine angle, a hard coating and a PTFE layer are added, and finally the strip is cut into individual blades, which are packed or bent and fixed into cartridges. HENLI has supplied coil feed lines for razor blade strip punching.

01What a blade is made of

What razor blades are made of

A razor blade is a thin strip of hardened stainless steel with two finished edges and a pattern of punched holes.

1

The steelA hardenable martensitic stainless steel with roughly 13 % chromium and enough carbon to reach a high hardness. It is supplied as very thin, narrow, cold-rolled strip in coils.

2

The holes and slotsPunched into the strip. On a double-edge blade they locate it in the razor; on cartridge blades the strip is narrower and the punched features help fix it to its support.

3

The edgesGround and honed to a small angle, then coated with a hard layer such as chromium or diamond-like carbon and a thin PTFE film.

4

Two kinds of bladeDouble-edge blades are flat, with an edge on each long side. Cartridge blades are narrow single-edge strips, bent and welded or clipped into a cartridge.

Where HENLI fits

The coil line for the punching step: payoff, feeding or pulling, and rewinding.

Hardening, grinding, honing, coating and packing are specialist lines.

For the press, HENLI works with partner press makers such as GOANWIN.

A double-edge razor blade and the six steps that make itLeft: a double-edge razor blade in top view with its punched centre slot and the two ground cutting edges. Right: six steps from stainless strip to blade: strip, punch the slots and holes, harden, grind and hone both long edges, coat, and cut into blades. The punching step, the one on a coil-fed press line, is highlighted.A double-edge bladeOrange: punched on the press line, and the ground edgesCutting edgeground, honed and coatedCentre slot and holespunched from the coilSecond cutting edgeboth long sidesFrom strip to bladeThe coil line covers step 2; the strip stays in one piece until step 61 · StripStainless coil2 · PunchSlots and holes3 · HardenHeat, quench, temper4 · Grind and honeBoth long edges5 · CoatHard layer + PTFE6 · CutInto bladesA double-edge bladeOrange: punched slot, ground edgesEdges: ground, honed, coatedSlot and holes: punched from the coilFrom strip to blade1 · StripStainless coil2 · PunchSlots and holes3 · HardenHeat, quench, temper4 · Grind and honeBoth long edges5 · CoatHard layer + PTFE6 · CutInto blades
Simplified drawing of a double-edge blade. Cartridge blades are narrower and are bent and fixed to a support after step 6; the punching step and the coil line in front of it are the same idea.

02The six steps

The razor blade manufacturing process, step by step

Most of the work happens on the strip, which stays in one piece until the very end.

1

StripThin martensitic stainless strip arrives in coils, cold-rolled to an even thickness and slit to width.

2

PunchA press punches the slots, holes and the notches where the blades will later be separated, one pitch at a time in a progressive die. The strip is rewound.

3

HardenThe strip runs through a hardening line: heated, quenched (often below zero) and tempered, so it reaches a high hardness but stays tough.

4

Grind and honeBoth long edges are ground in several stages to a fine angle, then honed to a keen edge.

5

CoatA hard coating, such as chromium or diamond-like carbon, is deposited on the edges, then a thin PTFE layer for a smooth shave.

6

Cut and packThe strip is cut into blades at the punched notches. Double-edge blades are wrapped; cartridge blades are bent and fixed to their supports.

Front of a GCH-200 double servo feeder with its upper and lower feed rolls and strip guide
Feed rolls and strip guide on a GCH-200 double servo feeder.

03Why punch first

Why the strip is punched before it is hardened

The order matters: holes and slots are punched while the steel is still soft, and the strip is kept continuous.

1

Soft steel punches cleanlyBefore hardening the strip cuts with a clean edge and little punch wear. Hardened blade steel would crack the strip or wear the punches quickly.

2

One piece through the next linesHardening, grinding and coating run strip to strip. Keeping the punched strip continuous and rewinding it lets it go through those lines as a coil.

3

Pitch decides the bladeThe notches set where each blade is cut later, so the pitch must repeat stroke after stroke.

4

Surface countsScratches and roll marks on thin blade strip can remain after grinding and coating, so the line must guide the strip gently.

Warped blade blanks are a different problem, solved by leveling; see why stamped blades warp and servo feeding and leveling for blade stamping.

Strip guide head and guide rollers on the entry side of a GCH-200 double servo feeder
Strip guide head and guide rollers at the entry of a double servo feeder.

04The coil line

The coil line for razor blade strip

A razor blade strip line is short and simple. HENLI has supplied coil feed lines for razor blade strip punching; a typical line has four machines around the press.

1

Pallet decoilerA horizontal pallet decoiler lets the coil lie flat on a rotating pallet, so the thin strip unwinds without twisting or rubbing: 5–120 mm strip, 0–1.2 mm, coils of 500 to 2,000 kg, 0–30 m/min with a VFD and electronic tracker.

2

Leveler, if neededWhere coil set affects the punching, a 6-Hi thin strip leveler for 0.03–0.3 mm strip.

3

Press with the dieA high-speed precision press punches the pattern. For the press, HENLI works with partner press makers such as GOANWIN and can recommend one.

4

Servo pull feederA GCD high-speed servo feeder or a GCH double servo feeder after the die pulls the punched strip out, one pitch per stroke.

5

RewinderAn MT recoiler winds the punched strip back into a coil for hardening: 200 mm and wider, 500 kg to 3 t standard, 15 m/min. For small coils, a light reel such as the CR up to 100 kg.

Horizontal pallet decoiler with a flat rotating pallet and a loop sensor arm
Horizontal pallet decoiler: the coil lies flat and pays off on demand.
Compact pallet uncoiler paying off narrow, thin strip
A compact pallet uncoiler paying off narrow, thin strip.

05Pull, not push

Why the servo feeder pulls the strip out of the die

Thin, narrow strip is easy to pull straight and easy to buckle when pushed.

1

PushingA feeder in front of the die pushes the strip in. With very thin strip, any resistance in the die or the guides can bend it or make it buckle before it reaches the pilots.

2

PullingA servo feeder after the die grips the punched strip and pulls it through. The strip stays straight under light tension and the payoff only has to release it.

3

Pilot releaseThe feeder still opens its rolls while the die pilots locate the strip; see why a feeder needs pilot release.

4

Feed and pullSome lines use one servo feeder before the die and one after, the layout used on motor lamination lines; see double-servo feed lines.

More on the layout: thin strip buckling before the die and front feed and rear pull.

A HENLI high-speed double servo feeder handling thin, narrow pierced strip at a customer's press.

06Single or double servo

Single servo or double servo feeder

Both can pull blade strip. The choice depends on the press speed, the pitch and how the feeder is mounted.

GCD high-speed servo feederGCH double servo feeder
DriveOne servo motor, gear-driven rollsTwo servo motors, rigid cast body
Pitch settingTouchscreen, 0–9,999.99 mmTouchscreen stroke, feed angle and release angle
Reference figures±0.02 mm; for presses up to 600 RPMUp to 60 m/min; 0.2–2.0 mm reference thickness
PositionIn front of or after the dieFeed side or pull side, or one of each
Choose it whenA simpler layout at moderate speedHigh speed, heavy vibration, or a feed-and-pull line

If your strip is thinner than the GCH reference range, HENLI sets the rolls and the pressure for the actual strip; send a sample with the inquiry.

07Your blade strip

Work out the strip speed, the coil and the line

Enter your strip and blade pitch. The calculator shows how fast the strip moves against the payoff, the feeder and the rewinder, how many blanks one coil gives, and which machines cover it.

Try itBlade strip, coil and lineEnter the strip width and thickness, the blade pitch, the press speed and the coil weight. See the strip speed against the line, the blanks per coil, and the payoff, pull feeder and rewinder that cover it. The example values are a double-edge blade strip.
The blade strip in the die and the strip speedTop: the strip in top view with the punched blade pattern one pitch apart and the current stroke in orange. Bottom: the strip speed as a bar against the 15 m/min of the MT recoiler, the 30 m/min of the pallet decoiler and the 60 m/min of the GCH double servo feeder.Strip 22.0 mm · pitch 43.0 mm12.9 m/minthis stroke← pulled out, rewoundfrom the coil ←Strip speed against the line, m/minrecoiler 15decoiler 30GCH 60
Strip speed12.9 m/minPitch × SPM: the speed the payoff, the pull feeder and the rewinder must match
Blanks per coil137,283One coil runs 7.6 h at 18,000 blanks / hCoil length 5,903 m
Payoff and feederHorizontal pallet decoiler, 500 kg class: the coil lies flat, 0–30 m/minPull the strip out after the die: thin strip can buckle if it is pushed inGCD single servo or GCH double servo feeder: ±0.02 mm on the GCD, up to 60 m/min on the GCH. Strip under 0.2 mm: Henli sets the rolls and pressure for it, send a sample
Leveler and rewinderIf coil set shows, a 6-Hi thin strip leveler covers 0.03–0.3 mmA light reel, such as the CR (up to 100 kg), or an MT recoilerStrip 12.9 m/min, within the MT recoiler’s 15 m/min
Strip speed = pitch × SPM. Coil length = coil weight ÷ (7,700 kg/m³ × width × thickness); blanks per coil = coil length ÷ pitch; start-up loss ignored. Pointers follow the standard HENLI tables: horizontal pallet decoiler 5–120 mm, 0–1.2 mm, up to 2,000 kg, 0–30 m/min; GCH double servo feeder 0.2–2.0 mm reference thickness, up to 60 m/min; GCD servo feeder ±0.02 mm; 6-Hi thin strip leveler 0.03–0.3 mm; MT recoiler 200 mm and wider, 15 m/min.

08Quotation data

What to send for a razor blade strip line

A line is chosen from the strip and the die, not from the feeder width alone.

1

StripGrade and hardness, thickness and width, surface finish and how much marking is allowed.

2

CoilInner and outer diameter and weight, so the pallet decoiler and the rewinder can be sized.

3

Die and pressBlade drawing or strip layout, pitch, press model and target speed, and the pilot release angle.

4

After the dieRewound for hardening, or cut into blanks at the press; the floor space for the line.

Line checklist

Pallet decoiler sized to the coil.

Leveler only if coil set affects the punching.

Servo pull feeder after the die, or feed and pull.

Rewinder speed matched to the strip speed.

HENLI equipment

The coil line for razor blade strip

Each page has the specifications, photos and a quotation checklist.

?FAQ

Razor blade manufacturing questions

How are razor blades made?

Razor blades start as a coil of thin martensitic stainless steel strip. The strip is punched with the slots and holes the blade needs while it is still soft and in one piece, then hardened by heating, quenching and tempering. Both long edges are ground and honed to a fine angle, a hard coating and a thin PTFE layer are added, and the strip is cut into individual blades. Cartridge blades are then bent and fixed to their supports; double-edge blades are wrapped.

What steel are razor blades made from?

Most are made from a hardenable martensitic stainless steel with roughly 13 % chromium and enough carbon to reach a high hardness after quenching and tempering. The steel comes as very thin, narrow, cold-rolled strip in coils.

How are razor blades made so sharp?

By grinding the edges in several stages to a small included angle, then honing them, and finally adding a hard coating, such as chromium or diamond-like carbon, plus a thin PTFE layer that lowers friction on the skin. Punching only shapes the strip; the sharpness comes from the edge grinding and finishing.

Where does stamping come into razor blade manufacturing?

At the start. The slots, holes and notches are punched into the coil strip before it is hardened, while it is still soft enough to punch cleanly. The strip is pulled out of the die and rewound so it can go through hardening and grinding in one piece. This is the step a HENLI coil line covers.

Why pull the strip after the die instead of pushing it?

Thin, narrow strip can bend or buckle when it is pushed into a die. A servo feeder after the die pulls the punched strip out, so the strip stays straight under light tension; see thin strip buckling before the die and front feed and rear pull.

Single servo or double servo feeder for blade strip?

Both work. A GCD high-speed servo feeder sets the pitch on its touchscreen to ±0.02 mm. A GCH double servo feeder has a rigid body and two servo motors, runs up to 60 m/min and can be used on the feed side or the pull side. The press speed, the pitch and the strip decide.

What machines are used in razor blade manufacturing?

A strip punching line (decoiler, press with die, servo pull feeder and rewinder), then a hardening line, edge grinding and honing machines, coating equipment, and cutting, bending and packing machines. HENLI supplies the coil line for the punching step; for the press, HENLI works with partner press makers such as GOANWIN.

What should I send for a quotation?

The strip grade, thickness and width, coil weight and inner and outer diameter, the blade drawing or strip layout, the pitch, the press and its speed, and whether the strip is rewound or cut after the die.

Razor blade strip line

Send Your Strip and Blade Drawing

Send the strip grade, thickness and width, the coil size, the blade drawing or strip layout, the pitch and the press speed. HENLI will propose the pallet decoiler, servo feeder and rewinder for the line.