Fuse Holder Clip and Relay Terminal Stamping: Parts, Progressive Die and Coil Line
Fuse clips, relay contact springs and terminals are small, springy, conductive and made by the million from thin copper alloy strip. Here is which parts are stamped, how the die builds them, and the line from coil to reel.
Every fuse block holds its fuses in pairs of spring clips, and every relay switches its load through a stamped contact spring. These parts are small, but they are made by the million, from narrow copper alloy strip that marks, twists and springs back easily.
This guide covers the parts first: fuse holder clips and the stamped parts inside a relay. Then it follows the strip through the progressive die and the line that feeds it, from a flat pallet decoiler to a terminal reel or a scrap chopper. A calculator works out the strip speed, the parts per coil and the machines that cover your job.
Fuse holder clips and relay terminals are stamped from thin copper alloy strip in a progressive die. The coil lies flat on a horizontal pallet decoiler so the narrow strip unwinds without twisting; a roller, gear or servo feeder moves it one pitch per stroke and releases it for the die pilots. Station by station, the die pierces holes, notches the outline, forms the spring fingers or bends, and cuts the part off, or leaves it on the carrier strip to be wound onto a reel. Relay contact springs, fixed-contact terminals, coil pins, armatures and yokes are made the same way. HENLI has supplied coil feed lines for fuse holder clips, and the same line suits relay parts.
01The parts
Which parts this line makes
Fuse holder clips and relay parts belong to one family: small conductive parts with a spring or contact area, punched from narrow strip at high speed.
Fuse holder clipsPairs of spring clips that grip the end caps or blades of a fuse in a fuse block, panel holder or PCB holder. Usually tin-plated brass, copper alloy or phosphor bronze; some carry a stainless backup spring.
Fuse terminals and bladesThe terminals of fuse bases and the blades of blade fuses come off the same kind of line; see the fuse terminal stamping guide.
Relay contact springsThe moving blade that carries the contact. Phosphor bronze or beryllium copper, chosen for spring life.
Relay terminals and pinsFixed-contact terminals and coil pins that pass through the relay base to the PCB, often pre-plated copper alloy or brass.
Armature and yokeThe magnetic parts of a relay, stamped and bent from soft iron strip.
Narrow, thin strip: often under 1 mm and under 100 mm wide.
Short pitch and high press speed.
A contact or spring area that must not be marked, bent or work-hardened by the line.
02The fuse clip die
How a fuse holder clip is stamped
A fuse holder clip is made in a progressive die: each station does one operation, and the strip carries the part from station to station.
Pilot holesThe first station punches holes in the carrier edge. Every later station has pilots that drop into them to locate the strip.
PierceWindows, slots and holes are punched while the strip is still flat.
Notch the outlineThe material around the clip is cut away, leaving it joined to the carrier by small bridges.
FormThe spring fingers are bent up and curled in; contact areas may be coined or embossed.
Cut off or keepThe clip is cut free and drops into a bin, or stays on the carrier and is wound onto a reel for plating or automatic assembly.
For the pilots to locate the strip, the feeder has to let go at the right moment; see why a feeder needs pilot release.
03Inside a relay
The stamped parts of a relay
Open a standard PCB relay and almost all the metal inside came off a coil: only the coil winding and the core are made another way.
Contact springStamped with its spring section and the hole for the contact rivet. Its flatness and temper set the contact force.
ContactsSilver-alloy contacts are riveted or welded onto the spring and the fixed terminals, in a dedicated die station or on a separate machine.
Fixed-contact terminalsStamped and bent so the contact sits in exactly the right place above or below the moving contact.
Coil terminalsStraight pins, usually from pre-plated strip, so the plating and the pin straightness both matter.
Armature and yokeSoft iron parts: the pole faces must stay flat, so the strip must be flat before it enters the die.
Winding the coil, molding the base and cover, and assembling and testing the relay are other machines.
This guide covers the strip stamping. For contact strip that needs leveling, oiling and slug removal, see the electrical contact strip guide.
| Relay part | Typical strip | What the line must protect |
|---|---|---|
| Contact spring | Phosphor bronze, beryllium copper | Spring temper, flatness, the contact area |
| Fixed-contact terminal | Copper alloy, brass | Contact position, burr direction |
| Coil terminal / pin | Brass or copper alloy, often pre-plated | Plating, pin straightness |
| Armature | Soft iron | Flat pole face |
| Yoke / frame | Soft iron | Bend angle, flatness |
04Strip and surface
Copper, brass and bronze strip, and how to keep it clean
These parts are chosen for conductivity and spring, and both suffer if the line marks or bends the strip.
Roll pressureEnough to feed without slipping, not so much that it prints the strip.
Roll surfaceClean rolls; polyurethane-covered rolls where bright or plated strip marks easily. For leveling, see leveling copper strip without roller marks.
GuidesSide guides that guide the strip without squeezing the edge or rubbing the contact zone.
Oil filmOnly as much oil as the die needs: a gravity-feed roller oiler or a pneumatic recirculating roller oiler puts a thin, even film on both faces; see the copper terminal strip oiling case.

| Strip | Line risk | What to confirm |
|---|---|---|
| Soft copper alloy | Dents, roller marks, edge rub | Roll pressure, guide shape, coil tension, threading path |
| Brass or bright plated | Scratches, roller pressure bands | Clean rolls, guide contact, whether oil is allowed |
| Phosphor bronze, beryllium copper | Springback, coil set | Straightening, pilot release, forming stations, temper |
| Stainless spring strip | Higher forming force, scoring | Leveling, die clearance, oil, roll grip |
05Why they are hard
Why fuse clips and relay terminals are hard to stamp
The parts look simple. The difficulty is keeping thin strip stable at high speed.
TwistThin, narrow strip twists before it reaches the die if the coil tension is unstable.
Short pitchA short pitch at high SPM leaves the feeder little time to feed and release.
Pilot fightIf the feed rolls still clamp the strip when the pilots enter, the pilots fight the feeder: holes move, punches wear, the feeder alarms.
Burr directionBurrs on slots, holes and contact faces must face the way the assembly needs.
SpringbackFormed fingers spring back after release, so the die and the strip temper must match.
Feed pitch variation is often blamed on the feeder, but it can start at the decoiler loop, the roll pressure or the strip flatness.
Check the whole path, from coil to scrap, before changing the die.
06The coil line
The line from coil to press
A typical line for fuse holder clips or relay terminals has four to six machines in a short row.
Pallet decoilerA horizontal pallet decoiler lets the coil lie flat and pays it off on demand: 5–120 mm strip, 0–1.2 mm, coils of 500 to 2,000 kg, 0–30 m/min with a VFD and electronic tracker. For small coils up to 100 kg, a CR light decoiler.
Leveler, if neededWhere coil set or springy strip affects the part, a precision leveler before the feeder.
OilerA roller oiler between the feeder and the die, where the die needs oil.
FeederAn RFS roller feeder, a GCF gear feeder or an NC servo feeder: chapter 07 compares them.
PressA high-speed precision press with the progressive die. For the press, HENLI works with partner press makers such as GOANWIN and can recommend one.
After the dieA terminal rewinder for strip on reels, or a scrap chopper and a bin for loose parts: chapter 09.
07Which feeder
Roller, gear, gripper or servo feeder
The feeder is chosen by the pitch, the press speed and how often the die changes, not by its name.
The RFS and GCF are driven by the press, so their feed is locked to every stroke; the HG grips the strip instead of rolling it; the NC servo feeder takes the press signal and feeds the length entered on its screen. For electronic springs and contact clips on a CR decoiler and roller feeder, see the electronic spring stamping line.
| Feeder | Pitch | Speed | Strip | Best for |
|---|---|---|---|---|
| RFS roller | Up to 300 mm by series | Up to 500 SPM | 100–700 mm, 0–3.5 mm | One fixed pitch, long runs |
| GCF gear | 12–250 mm by gear pair | 600–800 SPM by model | 150–300 mm, 0.1–1.0 mm | Thin strip, highest speed, ±0.02 mm |
| HG gripper | Up to 80 mm | Up to 800 SPM | 8–150 mm, 0.04–2.0 mm | Short pitch, narrow, delicate strip |
| NC servo | Set on the touchscreen | By pitch and press | By series | Many dies and pitches, frequent change |
08Your strip and line
Work out the strip speed, the coil and the line
Enter your strip and die. The calculator works out how fast the strip moves, how many parts one coil makes and how long it runs, and points to the decoiler, the feeder and what happens after the die.
09After the die
Carrier strip, loose parts and scrap
What leaves the die decides the last machine in the line.
Parts kept on the carrierA terminal rewinder winds the strip onto a reel with paper between the layers: the HT / DHT horizontal rewinder holds 20 kg per reel up to Φ650 mm and runs up to 20 m/min; the VT / DVT vertical rewinder where a vertical reel suits the space.
Loose partsParts drop through the die or slide down a chute into a bin; formed contacts should not fall onto each other.
Skeleton and carrier scrapA scrap chopper cuts the skeleton into short pieces, about 70 cuts per minute on the standard fixed-speed model; see terminal strip scrap handling and chopper or recoiler.
SlugsSmall slugs that stay in the die mark the strip and break punches; a scrap suction unit or a chute takes them away.
10Problems and quote data
Common problems, and what to send for a quotation
Feed pitch variation, poor pilot entry, deformed clips, scratched contacts and scrap jams are line problems as often as die problems. Run the line slowly and check in this order:
CoilDoes the strip leave the coil smoothly, in a relaxed loop?
EntryDoes it enter the leveler and the feeder square, without the guides squeezing it?
RollsIs the roll pressure right and the roll surface clean?
ReleaseDo feed completion and pilot release happen before the pilots enter?
DieAny slug pull-up, scrap jam or punch wear?
ExitDo the carrier strip and parts leave the die without pulling back on the strip?
Material, temper, thickness and width; plated or bare.
Coil weight, inner and outer diameter.
Part drawing, strip layout, pitch and parts per stroke.
Press, target SPM and pilot release method.
Parts on a reel or loose; scrap type; floor space.
For connector and automotive terminals on wider, faster lines, see the terminal stamping line guide.
HENLI equipment
The line for fuse clips and relay terminals
Each page has the specifications, photos and a quotation checklist.
?FAQ
Fuse clip and relay terminal stamping questions
How are fuse holder clips made?
Fuse holder clips are stamped from thin copper alloy, brass or phosphor bronze strip in a progressive die. The coil unwinds from a flat pallet decoiler, a roller, gear or servo feeder moves the strip one pitch per stroke, and the die pierces pilot holes and windows, notches the outline, forms the spring fingers and cuts the clip off, or leaves it on the carrier strip to be reeled for plating or assembly.
How are fuses made?
A cartridge fuse is a ceramic or glass tube with a fusible element inside, closed by metal end caps and often filled with quartz sand. A blade fuse has its element and both blades stamped from one piece of metal strip and molded into a plastic housing. The metal parts, from elements and blades to end caps and the clips of the fuse holder, are stamped or drawn from strip; the line in this guide makes the clips and terminals.
Which parts of a relay are stamped?
In a typical electromechanical relay, the contact spring, the fixed-contact terminals, the coil terminals or pins, the armature and the yoke are all stamped from strip. The silver contacts are riveted or welded onto the spring and the terminals. The coil, the core winding, the plastic base and the cover are made by other processes.
Which feeder is best for relay terminal progressive stamping?
For one fixed pitch up to 500 SPM, an RFS roller feeder (100–700 mm wide, pitch up to 300 mm). For thin strip at 600–800 SPM, a GCF gear feeder (150–300 mm, 0.1–1.0 mm, 12–250 mm pitch by gear pair) or, for short pitches on narrow strip, an HG gripper feeder. Where the die and the pitch change often, an NC servo feeder. The calculator above gives a first pointer.
Why does thin copper strip need low-tension decoiling?
Narrow, thin strip twists, drifts sideways or stretches when the feeder has to pull it off a heavy coil. A horizontal pallet decoiler lets the coil lie flat and pays it off on demand with a VFD and an electronic tracker, so the strip arrives at the feeder in a relaxed loop.
How can a stamping line reduce scratches on plated terminals?
Use clean rolls, polyurethane-covered feed rolls where the strip marks easily, only as much roll pressure as feeding needs, side guides that guide without squeezing, a measured oil film, a threading path without sharp bends or floor contact, and part collection that does not drop formed contacts onto each other.
Does HENLI make the stamping press?
HENLI builds the coil handling and feeding equipment: decoilers, levelers, feeders, oilers, terminal rewinders and scrap choppers. For the press, HENLI works with partner press makers such as GOANWIN and can recommend a suitable model for the die.
What data is needed before quoting a fuse holder clip stamping line?
Material and temper, thickness, strip width, plated or bare surface, coil weight, inner and outer diameter, the part drawing and strip layout, feed pitch, target SPM, the press, how the die releases the pilots, whether the parts stay on the carrier or drop loose, and the floor space.
Send Your Strip Layout and Coil Data